The Critical Balance: Holding Pressure & Time in Injection Molding
Published 1ย month ago
Description
Incorrect holding pressure and time can lead to critical defects like sink marks, warping, or short shots in injection molded parts. This episode breaks down the science behind these crucial parameters, their impact on part quality, and how to set them for optimal results.
Key Highlights:
- HOLDING PRESSURE ROLE: Holding pressure compensates for solidification shrinkage after mold filling, preventing voids and ensuring part strength and density.
- TRANSITION POINT: This critical moment shifts from injection to holding pressure, typically when the mold cavity is 95% filled.
- PRESSURE DEFECTS: Too low holding pressure causes short shots and sink marks, while too high pressure leads to warping, flash, and residual stress.
- HOLDING TIME EFFECTS: Insufficient holding time results in shrinkage dents and voids; excessive time prolongs cycle and can cause internal stress or gate protrusion.
๐ Read the Full Technical Guide: https://firstmold.com/guides/holding-pressure-and-holding-time/